Ukumelana nokushisa okuphezulu, ukukhanya okuphezulu, ukumelana nokushisa okuhle, kanye nokucutshungulwa okuhle kakhulu kwe-extrusion nokubunjwa komjovo.
Isetshenziswa kakhulu emikhiqizweni efana nekhabethe lesiqandisi.
In 25kg isikhwama esincane, 27MT nge Pallet
Iyunithi
Inkomba
Indlela yokuhlola
Melt Mass-Flow Rate
g/10 min
200℃×5kg
2.6
I-Izod Impact Amandla
kJ/m2
23℃,4mm,Notched
1.9
Charpy Impact Amandla
23℃,4mm
7.5
Amandla Okuqina
I-MPa
I-Tensile Modulus
I-Tensile Elongation
%
Amandla e-Flexural
I-Flexural Modulus
I-Vicat Softening Point
℃
I-Redual Monomer
ppm max
Ukuvutha
/