    Incazelo

    I-M500026T iyibanga le-Linear Low Density Polyethylene elinokusabalalisa kwesisindo se-molecular elifanele ukusetshenziswa kokusebenza komjovo. Iklanyelwe ukunikeza izakhiwo ezinhle kakhulu zokugeleza ezinokuqina okungcono kwezinga lokushisa eliphansi, ukumelana nokuqhekeka kwengcindezi kanye nokucwebezela.

    Amanani Ezakhiwo Ajwayelekile

    IZIMPAHLA IZIMALI EZIJWAYELEKILE AMANYE IZINDLELA ZOKUHLOLA
    IMPAHLA YEPOLYMER   
    Ukuminyana 926 kg/m³ I-ASTM D1505
    I-Melt Flow Rate (MFR)   
    ku-190 ℃ kanye no-2.16 kg 50 g/10 imiz I-ASTM D1238
    IZIMPAHLA ZEMITHETHO   
    Amandla e-Flexural 9 I-MPa I-ASTM D790
    I-Flexural Modulus (1% Secant) 200 I-MPa I-ASTM D790 A
    I-Izod Impact Amandla 500 J/m I-ASTM D256
    Ukuqina (Shore D) 50 - I-ASTM D2240
    ESCR (10% Igepal), F50 3 Hs I-ASTM D1693B
    ESCR (100% Igepal), F50 6 Hs I-ASTM D1693B
    Ingcindezi yokuqina ekuvuneni (50mm/min) 10 I-MPa ISO 527-2 1A
    Ingcindezi yokuqina ngesikhathi sekhefu (5mm/min) 12 I-MPa ISO 527-2 1A
    Ukuqina kwengcindezi ngesikhathi sekhefu (5mm/min) >100 % ISO 527-2 1A
    IZIMPAHLA ZOKUSHISA   
    I-Vicat Softening Point 88 I-ASTM D1525
    I-Brittleness Temperature <-75 I-ASTM D746

    Izimo Zokucubungula

    Izimo ezijwayelekile zokucubungula ze-M500026T yilezi: Izinga lokushisa lomphongolo: 180 - 230°C Izinga lokushisa lesikhunta: 15 -60 °C Ukucindezela komjovo: 600 - 1000 Bar.

    Ukucatshangelwa Kwezempilo Nokuphepha Nezinyathelo Zokuqapha

    I-M500026T ifanele isicelo sokuxhumana nokudla. Ulwazi oluningiliziwe lunikezwa kuDashidi Yedatha Yezokuphepha Ezibalulekile futhi ukuze uthole ulwazi olwengeziwe oluthile sicela uthinte ummeleli wendawo we-SABIC ukuze uthole isitifiketi. ISICELO: Lo mkhiqizo awuhloselwe futhi akufanele usetshenziswe kunoma yimuphiizicelo zemithi/zokwelashwa.

    Isitoreji Nokuphatha

    I-polyethylene resin kufanele igcinwe ngendlela yokuvimbela ukuchayeka okuqondile elangeni kanye/noma nokushisa. Indawo yokugcina kufanele futhi yome futhi okungcono ingeqi ku-50°C. I-SABIC ngeke inikeze iwaranti ezimeni ezimbi zokugcina ezingase ziholele ekuwohlokeni kwekhwalithi njengokushintsha kombala, iphunga elibi kanye nokungenzi kahle komkhiqizo. Kunconywa ukucubungula i-PE resin phakathi nezinyanga ezingu-6 ngemva kokubeletha.