• head_banner_01

Idatha ye-LLDPE 218WJ

Incazelo emfushane:

Sabic Brand
LLDPE| Ifilimu MI=2
Kwenziwe eSaudi Arabia


  • Inani :1100-1600 USD/MT
  • Imbobo :Xingang, Qingdao, Shanghai, Ningbo
  • I-MOQ:17MT
  • Inombolo ye-CAS:9003-53-6
  • Ikhodi ye-HS:390311
  • Inkokhelo :TT, LC
  • Imininingwane Yomkhiqizo

    Incazelo

    I-218WJ iyibanga lamahhala le-Butenear Low Density Polyethylene TNPP elifanele ukupakishwa kwenjongo evamile. Kulula ukucubungula ukunikeza izakhiwo ezinhle eziqinile, amandla omthelela kanye nezakhiwo ze-optical. I-218WJ iqukethe izithasiselo ze-slip kanye ne-antiblock.

    Izakhiwo

    Ifilimu yokugcoba, omalayini abancane, izikhwama zokuthenga, izikhwama zokuthwala, izikhwama zikadoti, amafilimu ahlanganiswe ndawonye, ukupakishwa kwabathengi nezinye izinhlelo zokusebenza ezijwayelekile.

    IZIMPAHLA IZIMALI EZIJWAYELEKILE AMANYE INDLELA YOKUHLOLA
    IMPAHLA YEPOLYMER
    Melt Flow Rate
    ku-190°C no-2.16 kg 2 g/10 imiz I-ASTM D1238
    Ukuminyana 918 kg/m³ I-ASTM D1505
    UKWENZIWA
    I-ejenti yokushelela - Indlela ye-SABIC
    I-ejenti ye-anti block - Indlela ye-SABIC
    IZIMPAHLA ZOKUBONA
    Inkungu 13 % I-ASTM D1003
    Ukucwebezela      
    ngo 60° 80 - I-ASTM D2457
    IZIMPAHLA ZIFILIMU
    I-Tensile Properties
    ukucindezeleka ngesikhathi sekhefu, MD 35 I-MPa I-ASTM D882
    ukucindezeleka ngesikhathi sekhefu, TD 29 I-MPa I-ASTM D882
    ubunzima ngesikhathi sekhefu, MD 700 % I-ASTM D882
    ubunzima ngesikhathi sekhefu, TD 750 % I-ASTM D882
    ukucindezeleka ngesikhathi sokuvuna, MD 12 I-MPa I-ASTM D882
    ukucindezeleka ngesikhathi sokuvunwa, TD 10 I-MPa I-ASTM D882
    1% secant modulus, MD 220 I-MPa I-ASTM D882
    1% secant modulus, TD 260 I-MPa I-ASTM D882
    Ukumelana nokubhoboza 63 J/m Indlela ye-SABIC
    Amandla Omthelela we-Dart 85 g I-ASTM D1709
    Elmendorf Tear Amandla
    MD 130 g I-ASTM D1922
    TD 320 g I-ASTM D1922
    IZIMPAHLA ZOKUSHISA
    I-Vicat Softening Point 98 °C I-ASTM D1525

    (1) Izakhiwo zikagesi zikalwe ngokukhiqiza ifilimu engu-30 μ ene-2.5 BURuses 100%218NJ.

    Izimo Zokucubungula

    Izimo ezijwayelekile zokucutshungulwa kwe-218WJ yilezi: Izinga lokushisa elincibilikayo: 185 - 205°C, isilinganiso sokuqhumisa: 2.0 - 3.0.

    Imithetho Yokuthintana Nezempilo, Ukuphepha Nokudla

    I-resin engu-218WJ ifanele isicelo sokuxhumana nokudla. Ulwazi oluningiliziwe lunikezwa kuDashidi Yedatha Yezokuphepha Ezibalulekile futhi ukuze uthole ulwazi olwengeziwe oluthile sicela uthinte ummeleli wendawo we-SABIC ukuze uthole isitifiketi. ISIVIVINYO: Lo mkhiqizo awuhloselwe futhi akufanele usetshenziswe kunoma yiziphi izinhlelo zemithi/zezokwelapha.

    Isitoreji Nokuphatha

    I-polyethylene resin kufanele igcinwe ngendlela yokuvimbela ukuchayeka okuqondile elangeni kanye/noma nokushisa. Indawo yokugcina kufanele futhi yome futhi kungcono ingeqi ku-50°C. I-SABIC ngeke inikeze iwaranti ezimeni ezimbi zokugcina ezingase ziholele ekuwohlokeni kwekhwalithi njengokushintsha kombala, iphunga elibi kanye nokungenzi kahle komkhiqizo. Kunconywa ukucubungula i-PE resin phakathi nezinyanga ezingu-6 ngemva kokubeletha.